Alma Posted August 11, 2011 Report Share Posted August 11, 2011 Hello, I am looking for a white slip recipe I could use for painting over with iron oxides. The clay that I work with is a low fire terracotta. Also, any simple white glaze recipes - gloss or semi-matte- would be very much appreciated. Alma Link to comment Share on other sites More sharing options...
bciskepottery Posted August 13, 2011 Report Share Posted August 13, 2011 These slip recipes were posted on the NC Clay Club blog site and may be helpful. http://itc.utk.edu/web/Brogden/ceramics_website/final_pf_files_3_5/slips.pdf Link to comment Share on other sites More sharing options...
Alma Posted August 14, 2011 Author Report Share Posted August 14, 2011 Thank you so much for this wonderful recipe collection, bciskepottery! I'll definitely give them a try. Link to comment Share on other sites More sharing options...