Thrown; yakishime; youhen charcoal finish; noborigama woodfired at Kanayamayaki, Goshogawara-shi, Aomori-ken, Japan; Orton cone 14. Private collection in Japan.


Copyright

© John Baymore 2013 - all rights reserved
Sign in to follow this  
From the album:

John Baymore's Clay Work

  • 31 images
  • 0 comments
  • 38 image comments

Photo Information for Youhen Flower Arranging Vase

Taken with Canon Canon PowerShot SX160 IS

  • 15.9 mm
  • 1/4
  • f f/8.0
  • ISO 100
View all photo EXIF information

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.