I have a whole bunch of Buff Continental Clay that I purchased for a good price and I have been using Mayco premixed glazes and most seem to craze with the except maybe three. I apply thin coats and I don’t shock them either. I dont want to start mixing my own glazes because I dont have the time or the money to invest in that. Could someone help me out in suggesting some glazes that work well with this clay?