I am looking to add color to the foot ring after firing cone 6 white porcelain. Looking to make the foot ring black. Any recommendations as to what to use? Have tried India Ink, black shoe polish, black shoe dye. So far of these the black shoe dye looks the most promising. Also considering black underglaze, although it wold not be fired. Any recommendations would be appreciated. Thanks
Coloring unglazed porcelain foot ring
in Clay and Glaze Chemistry
Posted
Also considering black stove polish