8 hours ago, neilestrick said:
What brand and model of clay is it? What cone are you firing to?
It’s Sio-2 PRNI black stoneware, firing to come 5 or 6. But the chalkiness is happening before firing, just as it dries normally.
-
I have this black stoneware clay that has been drying and firing really light. It almost looks chalky when it’s dry. Even after it’s fired it’s still chalky and like it has a dusty white tinge to it. It is very dark when wet, and the first time I used it the Color was very dark after firing. Any insight into how or why this changed? Or how to fix it?
Black stoneware look chalky when dry
in Clay and Glaze Chemistry
Posted
Not sure about the glaze firing, I have not gotten that far yet. I’ll be running the kiln in a few days hopefully and then I’ll be able to see if this batch bisque fires chalky as well.