Hello- I have an older model 181 Skutt kiln- I just ran my first cone 6 kiln and it shut off- tripped the breaker within 20 minutes. . On the top shelf one piece exploded. But the rest survived. Also on top the cone holder turned black along with the cones. Can someone please help with advice? Thank you so much!
Skutt model 181 kiln?
in Equipment Use and Repair
Posted
Hello- I have an older model 181 Skutt kiln- I just ran my first cone 6 kiln and it shut off- tripped the breaker within 20 minutes. . On the top shelf one piece exploded. But the rest survived. Also on top the cone holder turned black along with the cones. Can someone please help with advice? Thank you so much!