Report Is there a way to repair bisque pottery without re-firing? in Studio Operations and Making Work Posted February 7, 2023 Maybe something like patch-a-tatch https://bigceramicstore.com/products/duncan-patch-a-tatch
Report Is there a way to repair bisque pottery without re-firing? in Studio Operations and Making Work Posted February 7, 2023 Maybe something like patch-a-tatch https://bigceramicstore.com/products/duncan-patch-a-tatch
Is there a way to repair bisque pottery without re-firing?
in Studio Operations and Making Work
Posted
Maybe something like patch-a-tatch
https://bigceramicstore.com/products/duncan-patch-a-tatch