I tried doing my first bisque firing in my American Beauty AB18 kiln. It got up to 1100° F with 3 out of 4 switches on, so I flipped the 4th/top switch on. At next check, an hour later, the indicator light was off and I'd lost 200 degrees. What might have happened? It didn't trip the circuit breaker. It won't turn on now.
First Bisque Firing Failure - Troubleshooting
in Equipment Use and Repair
Posted
I tried doing my first bisque firing in my American Beauty AB18 kiln. It got up to 1100° F with 3 out of 4 switches on, so I flipped the 4th/top switch on. At next check, an hour later, the indicator light was off and I'd lost 200 degrees. What might have happened? It didn't trip the circuit breaker. It won't turn on now.