I realize this problem is a result of my port planning, but…I am trying to fulfill a wholesale order and need standard white stoneware 630, but the supply store I typically use is out of stock. I have a deadline and need the clay asap. To fulfill the rest of order and make it consistent with prior glaze results I need that clay or something very similar. Does anyone have a recommendation for a very similar clay that may have similar glaze results? Or does anyone in Chicago area have just 25lbs of 630 to sell to me?
Alternative to standard 630
in Clay and Glaze Chemistry
Posted
Thanks all! Ceramic supply Chicago is my usual supplier who is out of stock. I did contact them about a possible substitute and they recommended 240 or 182 with no guarantees, of course. I’m going to try 240g and hope for the best!! Thanks everyone.