32 minutes ago, oldlady said:
yep, the early version looked like that. pinky, where is lithgow? cannot imagine where you are if you do not say so.
Lithgow is a small city in NSW, Australia!
-
2 hours ago, Babs said:
Get it tested but looks like early ceramic fibre, asbestos not used like that for many decades. Ceramic fibre not to be used casually either, very bad if inhaled and irritates the skin. Can get a spray but better to replace with ceramic board.
Use a mask near that puppy.
What are the specis on your kiln? Date etc Manufacturer could give info you need.
The asbestos/ ceramic fibre top looks like a home jobbie to replace a faulty top., the sag is greatly reducing your interior space.
Check all other stuff needing work. Could get expensive.
The kiln was very cheap so I am happy to spend a little bit to get it in good working order. Thanks for the information and advice!
-
-
Thanks so much. Ill get a sample sent off in the next few days. Do you by any chance know if the insulation can be changed or if it renders the kiln useless?
-
Asbestos
in Equipment Use and Repair
Posted
Thank you! I sent a sample off to be tested today!