Hello, I am a ceramics instructor and I have been making ceramics for over 30 years. I use Laguna clay. Recently I have a new issue with their bmix. I am having over 1/2 of my handles on my mugs crack at the join. This has never happened before. I dry extremely slowly. In magic boxes for over a week then in plastic wrap for over a week. I never used slip with vinegar before but tried it when this started happening and it still cracks. I also never waxed my handles but tried that as well. Is anyone else having issues? Or does anyone have any suggestions? Did they change their recipe?
Handle cracking question
in Studio Operations and Making Work
Posted
I will post the next batch of mugs. I smashed the last ones.
Thanks though.