Report 2 segment firing schedule in Clay and Glaze Chemistry Posted July 4, 2022 Hello everyone, I recently got a pottery crafts aurora kiln and I need a good 2 segment firing schedule. i contacted the company for one but my pieces came out under fired (I use HF amaco glazes) my program was 1) 60 Celsius to 600 soak for 10 2) then 120 to 122 and soak for 10 mins anyone recommend another firing schedules for cone 5 or 6 for me to try out? Or should I just make the second soak longer?
2 segment firing schedule
in Clay and Glaze Chemistry
Posted
Hello everyone,
I recently got a pottery crafts aurora kiln and I need a good 2 segment firing schedule.
i contacted the company for one but my pieces came out under fired (I use HF amaco glazes)
my program was
1) 60 Celsius to 600
soak for 10
2) then 120 to 122
and soak for 10 mins
anyone recommend another firing schedules for cone 5 or 6 for me to try out? Or should I just make the second soak longer?