Well the title says it all... i tried a piece of foil on the top and the difference in temperature felt with my hand is impressive... i am tempted to cover the whole lid... the brick underneath seems hotter too. I am guessing there is perhaps a reason not to do that, what do you think?
using aluminum foil over kiln lid to reduce radiant heat loss.... could it?
in Equipment Use and Repair
Posted
not getting a crack in the lid is worth not doing that... might think a little longer before trying... thank you for your answers!