Hi, thanks everyone.
In answer to your questions:
1. Firing to 1240
2. Oxidation in electric kiln
3. G72150 multi-purpose stoneware transparent glaze, firing range 1200 - 1290
4a. I first used Mason Peacock 6266 at 8% (with the china clay/ ball clay slip - oh, also with a little feldspar potash, recommended by the supplier)
This resulted in a very dark blue - could I rectify this by just diluting it with more of the ball/china/little bit of potash clay slip?
4b. Then I used Mason Deep Turquoise 6315 at 8% (with the more complicated slip)
I was advised to add the feldspar potash and the silica by the supplier that I bought the stains from, but it resulted in a very washed out anaemic blue instead of the deep turquoise.
I imagine I should just forget about the complicated slip?
Am I still ok using the ball clay/china clay/little bit of potash slip with the stoneware (I have mixed up quite a bit)?
Would there be any difference between using this and a slip made from the white stoneware clay?
I'm after a pure colour, as shown on the Mason stains chart.
Thanks again!
-
Hi, thanks everyone.
In answer to your questions:
1. Firing to 1240
2. Oxidation in electric kiln
3. G72150 multi-purpose stoneware transparent glaze, firing range 1200 - 1290
4a. I first used Mason Peacock 6266 at 8% (with the china clay/ ball clay slip - oh, also with a little feldspar potash, recommended by the supplier)
This resulted in a very dark blue - could I rectify this by just diluting it with more of the ball/china/little bit of potash clay slip?
4b. Then I used Mason Deep Turquoise 6315 at 8% (with the more complicated slip)
I was advised to add the feldspar potash and the silica by the supplier that I bought the stains from, but it resulted in a very washed out anaemic blue instead of the deep turquoise.
I imagine I should just forget about the complicated slip?
Am I still ok using the ball clay/china clay/little bit of potash slip with the stoneware (I have mixed up quite a bit)?
Would there be any difference between using this and a slip made from the white stoneware clay?
I'm after a pure colour, as shown on the Mason stains chart.
Thanks again!