Report A used Bluebird 12 Clay Mixer? in Equipment Use and Repair Posted August 23, 2022 I have an old Bluebird pugmill which is about 20 years old. Little bits of metal are getting into the clay. No idea where it’s coming from.
A used Bluebird 12 Clay Mixer?
in Equipment Use and Repair
Posted