    jojess got a reaction from Rae Reich in Large Flat Pieces Cracking During Glaze Firing   
    Hi Karen,  thank you for your hints and tips..i used grog on my shelves for the first time and no cracks in my hearts  yay!!  I am now trying paperclay, rather than the porcelain that i have been using as someone suggested that it maybe more suited to my flat pieces.  I have some more hearts drying so yet to see what they will do in the first firing.
  2. Like
    jojess reacted to Karen B in Large Flat Pieces Cracking During Glaze Firing   
    Hi Karen,  thank you for your hints and tips..i used grog on my shelves for the first time and no cracks in my hearts  yay!!  I am now trying paperclay, rather than the porcelain that i have been using as someone suggested that it maybe more suited to my flat pieces.  I have some more hearts drying so yet to see what they will do in the first firing.
     
     That sounds like a good idea Jo. Let us know how it works. 
  3. Like
    jojess got a reaction from jrgpots in Large Flat Pieces Cracking During Glaze Firing   
    Hi Benzine,  wow there are helpful people on this site , this is the first time that i have asked a question and am so thankful that people are happy to offer advise.  I did change the shape of the heart so there is a softer angle at the top and not a sharp 'V' but some of them still crack.  I am handcutting them so is this the problem??  should i lift them off the shelf with stilts, i am just worried about sagging tho.
×
×