gjt
-
Posts
2 -
Joined
-
Last visited
Content Type
Profiles
Forums
Gallery
Status Updates posted by gjt
-
I tried the Nutmeg ^6 glaze from Ceramics Monthly a while back, but my results look NOTHING like the picture! It's not that rich deep orange, but rather a mottled yellow-orangish color. Am I missing something? (I fire a little hotter than ^6, sometimes a slow cool-- for mattes, etc.-- and sometimes not.)