In addition to finding out if, or how much, the glaze will run, the test tiles will let you see what the glazes look like without the reduction that takes place in raku process.. There's a good chance that without that step, they're going to look a lot different than expected - and your student may decide they don't like the results well enough to use it on the pieces they originally planned.