Hello. I recently replaced my original thermocouple in my 15+ year old Skutt 1018KM because of an overfired glaze firing( yes witness cones used). In my next bisque(04), it was underfired though reached temp according to controller. Solutions please. The elemts are original as well. I generally fire Bisque 04 and Glaze Cone 5 with 15 min hold. Thank you!
Calibrate new Thermocouple or change old elents
in Equipment Use and Repair
Posted
Hello. I recently replaced my original thermocouple in my 15+ year old Skutt 1018KM because of an overfired glaze firing( yes witness cones used). In my next bisque(04), it was underfired though reached temp according to controller. Solutions please. The elemts are original as well. I generally fire Bisque 04 and Glaze Cone 5 with 15 min hold. Thank you!