Jump to content
3Ni12Mno
 

3Ni12Mno

glazenerd
Sign in to follow this  

3% Nickel ox plus 1/2% manganese. Complete color shift, blue crystals not present.

Copyright

© TJA 2016
Sign in to follow this  
From the album:

Clay Tests

  • 35 images
  • 0 comments
  • 34 image comments

Photo Information for 3Ni12Mno

Taken with EASTMAN KODAK COMPANY KODAK EASYSHARE C182 Digital Camera

  • 5.7 mm
  • 16667/1000000
  • f f/8.8
  • ISO 80
View all photo EXIF information

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.