testfiring


Marcia Selsor
 Share


At 1500 the walls were warm ..felt like tepid bath water. Could rest my hand on the surface.2" of fiber insulation all the way around.

I like the results of this little kiln. Very light weight.Will weigh it.

From the album:

Kilns

  • 28 images
  • 0 comments
  • 9 image comments

Photo Information for testfiring

Taken with Apple iPhone 6

  • 4.2 mm
  • 1/879
  • f f/2.2
  • ISO 32
View all photo EXIF information
 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.