119 W Copper Carb cone10OX 800x magnified
clear glaze with copper carb cone 10 Oxidation. 800x magnified and backlit. The large measuring mark is a 1 millimetre mark, the small marks are one tenth of a millimetre. Bubbles are about one tenth of a millimetre and are not visible to the naked eye.