red porcelain coffee cup bottom at 200x magnification
these bubbles are definitely much more numerous, and somewhat larger than on the walls of the pot where the glaze was flowing well. This is a celadon glaze
these bubbles are definitely much more numerous, and somewhat larger than on the walls of the pot where the glaze was flowing well. This is a celadon glaze