Covered jar from the jacket of "Alabama Folk Pottery".

Cone ten. Stamped, stained, then wax resist over the stained stamps,

then glazed. I think it was made with 10 lbs clay.

See ya,

Alabama

Copyright

© Ali Bhama

From the album:

Alabama

· 32 images
  • 32 images
  • 0 comments
  • 12 image comments

Photo Information

  • Taken with Quanta QMV7a
  • Focal Length 2.8 mm
  • Exposure Time 0/0
  • f Aperture f/2.8
  • ISO Speed 200

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.