© Copyright 2015, Paul M. Chenoweth, Nashville, TN. All rights reserved.

Anthurium Couldn't Wait



I slipped this container into a tall spot in the kiln at the last minute to see how my glazes break over the undulating walls. Actually, I really needed the pot for the Anthurium that I received as a birthday gift back in January...it was quite root bound and begging for better living conditions.

 

Container is about 13" tall, stoneware, fired to cone 10 reduction and glazed with a combination of Ohio White, Woo's Blue, and Clear (sprayed on in overlapping layers).

Copyright

© Copyright 2015, Paul M. Chenoweth, Nashville, TN. All rights reserved.

From the album:

Tornado Pot Sketches and Progress Images

· 15 images
  • 15 images
  • 0 comments
  • 40 image comments

Photo Information


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.