Occasionally I need to burn up some brush, dead fall, etc. I thought why waste a perfectly good fire! These two pieces made from raku clay and bisqued at 04 electric. I coated them with some copper based raku glaze. While I was piling up the brush, I just placed these two pieces in the middle of the pile and lit it. I then spent the next couple of hours running around the yard for more deadfall to keep the fire going.
I got the pieces hot enough to melt the glaze and got a pretty good workout at the same time. Next time I'll try to have more burn stuff piled ready to go.
The are the results!