Occasionally I need to burn up some brush, dead fall, etc. I thought why waste a perfectly good fire! These two pieces made from raku clay and bisqued at 04 electric. I coated them with some copper based raku glaze. While I was piling up the brush, I just placed these two pieces in the middle of the pile and lit it. I then spent the next couple of hours running around the yard for more deadfall to keep the fire going.

 

I got the pieces hot enough to melt the glaze and got a pretty good workout at the same time. Next time I'll try to have more burn stuff piled ready to go.

 

The are the results!

Copyright

© © William Tucker 2014
From the album:

Williamt

  • 3 images
  • 0 comments
  • 0 image comments

Photo Information for Open Burn Raku

 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.