© © William Tucker 2012, 2014

reimagined



ok before your say craft or more "duckies and chickens" let me tell you about this.

Started as an exersize in clay shrinkage and designing to fit.

As we know, clays have different shrinkage numbers and temp certainly has an effect on that shrinkage.

The experiment started with just going by the shinkage numbers given with the clay body. I soon discovered that there is some deviation to that number (they should give the average shrinkage and an observed deviation). But I digress.

I liked the way they looked and they were different. So......

I measure the appropriate dimensions on the found glass objects, interesting things from thrift stores. I then throw a base and a lid, based on the glass dimension, plus the published shrinkage, plus a fudge factor that you have to determine with the clay you are using.

I bisque, the glaze, fire to cone 5 (stoneware). Usually now, I get a pretty good fit. Sometime the lid is a little big or small though. if I like the way the lid looks, I'll grind or add cork or foam filler.

I found that folk like and actually buy these. If you want more info, shoot me an emai.

Copyright

© © William Tucker 2012, 2014
From the album:

Williamt

  • 3 images
  • 0 comments
  • 0 image comments

Photo Information for reimagined


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.