Norm's Olive Speckle
Ferro Frit 5301 with 10% Nickel Carbonate and 1% Bentonite for ^06, add Silica and Kaolin for ^6
Photo Information
- Taken with Panasonic DMC-TS2
- Focal Length 4.9 mm
- Exposure Time 10/10000
- f Aperture f/3.3
- ISO Speed 80
Ferro Frit 5301 with 10% Nickel Carbonate and 1% Bentonite for ^06, add Silica and Kaolin for ^6