IMG 20130928 171145
Glaze fired vase. First experiment combining glaze and saggar firing. Fired first with a commercial glaze on the inside of the vase. Fired in an aluminum foil saggar a second time with ferric chloride, epson salt, horse hair, miracle grow, cobalt carbonate and copper carbonate. Successful test, sold within minutes of being finished.