The kiln collapse; I had moved the location of the base posts to fit a larger platter in that zone. Studio mate didnt notice the new layout when he loaded next, and this happened! These few pots kept the rest of the kiln from collapsing. Amazing since the kiln was at about cone 10-12 when the collapse occurred. Some Strong pots!