I want to start using Pilcher's slip on my sculptural pieces. It is a cone 04-10 recipe. What's the best plan to begin converting this into a vitreous recipe at cone 5/6?

Here's the recipe:

Ball clay 25, EPK 25, Flint 25, Cornwall Stone 12.5, Neph Sy 12.5

Add: Zircopax 5, Frit 3124 5

 