totemtina Posted May 15, 2015 Report Share Posted May 15, 2015 I want to start using Pilcher's slip on my sculptural pieces. It is a cone 04-10 recipe. What's the best plan to begin converting this into a vitreous recipe at cone 5/6? Here's the recipe: Ball clay 25, EPK 25, Flint 25, Cornwall Stone 12.5, Neph Sy 12.5 Add: Zircopax 5, Frit 3124 5 Thank you! Tina Link to comment Share on other sites More sharing options...
TJR Posted May 15, 2015 Report Share Posted May 15, 2015 Try replacing all of the Cornwall Stone with Neph Sy. Then you will have 25% Neph Sy. TJR. test,test,test. Link to comment Share on other sites More sharing options...