Dory709 Posted July 17, 2014 Report Share Posted July 17, 2014 When you are going for a marbled look by adding a mason stain to part of the clay, do you let the "dyed" clay sit for a period of time after mixing in the stain before wedging it? If not, should it sit before combining it with the other color clay? Thanks in advance. Link to comment Share on other sites More sharing options...
Chris Campbell Posted July 17, 2014 Report Share Posted July 17, 2014 No, it does not need to sit or age after the stain is mixed into the clay. I have a section of my website with lots of colored clay lessons. http://ccpottery.com/murrinis.html Link to comment Share on other sites More sharing options...