Autumn Joy Posted December 7, 2013 Report Share Posted December 7, 2013 I have a small collection of animal bones that I have found while out in the woods or on camping trips. I would like to incorporate them into some larger bowls that I have made by having the imprint of the bones to be visible. My professor suggested placing them at the bottom and pouring some glaze on top or sprinkling some wood ash. Wasn't sure if anyone else had experimented with this and had any helpful suggestions before I start. Link to comment Share on other sites More sharing options...