Hi,

Thanks for the replays to my question about what temp to fire pclay over metal. I fired a some pieces at 04 and one at 06. O4 pieces seemed to be more fragile. Now...can these pclay over metal be refired? If so, again to what temp.

I really like the forum. I think it would be great to have one just for paper clay.

Thanks

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,066 posts
  • LocationRaleigh, NC

Posted 27 September 2010 - 04:41 PM

Yes, you can fire them again ...
The limits on the temp would be decided by the melting point of your metal and the cone your clay fires to.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 acg

acg

    Member

  • Members
  • PipPip
  • 22 posts

Posted 27 September 2010 - 10:24 PM

Yes, you can fire them again ...
The limits on the temp would be decided by the melting point of your metal and the cone your clay fires to.