auroramoon Posted September 2, 2013 Report Share Posted September 2, 2013 Hi, Has anyone used the Mayco Copper Ore? I thought it would come out kind of metallic, but It ended up being just a boring matte brown. I painted it on, 2 coats. It was on 182 clay. Any suggestions? Should I put it on thinner, or use with another glaze? I wanted that nice metallic, bronzy-copper color. Help please! Link to comment Share on other sites More sharing options...