Posted 20 May 2013 - 05:52 PM

Would someone be so kind as to walk me through the making of colored clay preferably with already manufactured ingredients like mason stains. Some years back I tried adding the powdered stain directly into my clay body but with only minimal success... What has worked for you?

#2 AtomicAxe

AtomicAxe

    Skilled Mud Bug

  • Members
  • PipPipPip
  • 195 posts
  • LocationAmarillo, TX

Posted 20 May 2013 - 07:20 PM

When I color my clay, one of the easiest ways I usually do it is just to add the mason stains to my slip in my scrap buckets and blend in with a jiffy mixer. simple. When you reclaim as normal ... you have an easier time wedging.

#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,090 posts
  • LocationRaleigh, NC

Posted 20 May 2013 - 07:35 PM

Here is a link to my website where I show how to color clay with mason stains and how to use it.

http://ccpottery.com/murrinis.html

I have also written articles on it ... Check the January issue of PMI.
If you have further questions, just ask.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users