I have been experimenting with slip casting white clay bodies and I can't seem to make a slip that will work the way I want it to. Does anyone have a good cone 6 porcelain slip recipe that they use? I would like one that does not crumble when you cut it, so I can alter the lips of the pieces and also carve on them. Also, it does not have to be extremely transparent since I will be glazing the objects.

Thanks!

ceraymics likes this

Share this post


Link to post
Share on other sites

I'm looking for the same, but can't find anything that works at /\6 oxidation.

Have tried: 

grolleg        60

epk             60

flint             60

custer  feldspar 30

neph sye    30

bentonite     5

darvan

 

Fired at /\6-7 it remains porous.

 

Any help is appreciated.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×