New glazes I picked up:

 

Stellar Rust (I have used before)

Stormy Night

Caribbean

Nutmeg

 

These are glazes from Clay Art Centre in Tacoma, WA.

 

If anyone has experience with these and knows a (M50 cup) viscosity number start with please let me know.

 

The manufacturer will only tell me "medium cream" and "thin cream"

 

 

Thanks. B)

Share this post


Link to post
Share on other sites

Another glaze I mixed up today was some old MS34 Burnt Sienna. (2 kg dry)

I'm guessing that this is a Luguna product.

 

I mixed up the powdered glaze with a high speed blender for 5 minutes and transferred to another bucket through a sieve.

 

The amount of solids in the sieve was startling.

There was enough material in the sieve (maybe 500 - 600 grams) that I figure that it should be either in solution or a much finer particle in suspension.

 

Has anyone seen this occur with old glazes or this burnt sienna?

 

I put all of it back into the bucket and mixed another 5 minutes.

I will allow it to hydrate overnight and give it another mix in the morning.

 

:)

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×