Jump to content


Photo

Viscosity Recommendations


  • Please log in to reply
1 reply to this topic

#1 Mark McCombs

Mark McCombs

    Advanced Member

  • Members
  • PipPipPip
  • 123 posts
  • LocationSW Washington

Posted 05 November 2012 - 02:07 PM

New glazes I picked up:

Stellar Rust (I have used before)
Stormy Night
Caribbean
Nutmeg

These are glazes from Clay Art Centre in Tacoma, WA.

If anyone has experience with these and knows a (M50 cup) viscosity number start with please let me know.

The manufacturer will only tell me "medium cream" and "thin cream"


Thanks. B)
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt

#2 Mark McCombs

Mark McCombs

    Advanced Member

  • Members
  • PipPipPip
  • 123 posts
  • LocationSW Washington

Posted 05 November 2012 - 05:57 PM

Another glaze I mixed up today was some old MS34 Burnt Sienna. (2 kg dry)
I'm guessing that this is a Luguna product.

I mixed up the powdered glaze with a high speed blender for 5 minutes and transferred to another bucket through a sieve.

The amount of solids in the sieve was startling.
There was enough material in the sieve (maybe 500 - 600 grams) that I figure that it should be either in solution or a much finer particle in suspension.

Has anyone seen this occur with old glazes or this burnt sienna?

I put all of it back into the bucket and mixed another 5 minutes.
I will allow it to hydrate overnight and give it another mix in the morning.

:)
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt