Smoke and wood kiln

Recommended Posts

Mistelle    0

Bonjour !

 

During the firing of a wood kiln what color the smoke from the chimney should be ? Someone told me that a black smoke is the sign of humid wood. Is it true ?

 

Merci ! biggrin.gif

Share this post


Link to post
Share on other sites
TJR    359

I am going to jump in here, even though I am not an expert on wood firing. I have fired a few wood kilns around the world.

Black smoke is a sign of incomplete combustion. This is carbon burning off outside of the kiln. You want to time your stokes so that you get "some" smoke, but not black. I have never heard of this indicating damp wood. You could probably hear steam being given off if the wood is damp.

Of course you want to avoid damp wood, as this reduces the efficiency of your firing.

TJR

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×