Shino libbys base with a flat shaners red on top.




I wash of my bowls I take my time and prep them.  Wait for one to dry then dip it in the other. 




Any ideas on how to prevent more crawling or stop it? besides Kiln errors




Posted Image

#2 Matt Katz

Matt Katz

    Member

  • Members
  • PipPipPip
  • 50 posts
  • LocationAlfred, New York

Posted 09 June 2010 - 11:37 AM

Shino libbys base with a flat shaners red on top.

I wash of my bowls I take my time and prep them. Wait for one to dry then dip it in the other.

Any ideas on how to prevent more crawling or stop it? besides Kiln errors


Shinos crawl because of high clay content and shrinkage.
Adding darvan may reduce the problem.

#3 Monna

Monna

    Member

  • Members
  • PipPip
  • 13 posts

Posted 09 June 2010 - 09:45 PM


Shino libbys base with a flat shaners red on top.

I wash of my bowls I take my time and prep them. Wait for one to dry then dip it in the other.

Any ideas on how to prevent more crawling or stop it? besides Kiln errors


Shinos crawl because of high clay content and shrinkage.
Adding darvan may reduce the problem.