Jump to content


Photo

Bisque Firing For Air Drying Clay


  • Please log in to reply
2 replies to this topic

#1 katalayne

katalayne

    Newbie

  • Members
  • Pip
  • 4 posts

Posted 30 May 2010 - 08:58 PM

I am a newbie and just bought a kiln. I have some air dry clay that can be also be fired to cone 5-10. Do I need to fire initially to the bisque stage or go ahead after it is air dry and glaze and then fire it? Thanks for any assistance.

#2 kennwitt

kennwitt

    Newbie

  • Members
  • Pip
  • 4 posts

Posted 31 May 2010 - 12:47 PM

Hi you can do one firing but if you are new I would suggest you bisque fire your bone dryed clay to 04 then glaze and re-fire to the recomend cone of your glaze.

#3 katalayne

katalayne

    Newbie

  • Members
  • Pip
  • 4 posts

Posted 31 May 2010 - 01:43 PM

Hi you can do one firing but if you are new I would suggest you bisque fire your bone dryed clay to 04 then glaze and re-fire to the recomend cone of your glaze.