Kabe Posted October 28, 2011 Report Share Posted October 28, 2011 Is there a clay recipe that could be used for a cone 10 firing that would be suitable for reusable tile stands. They do not need to hold up a stack of shelves just indvidual pieces. So there is not a lot of wieght involved, but it would need to stay flat. The clay body I use now does not warp but I do not know if it is suitable to make furniture out of. I have some work that can not be fired flat like most tiles are. I would like to be able to fire something at a higher temp so it more like real kiln shelves as far as strength and resistace to heat. Any suggestions. Link to comment Share on other sites More sharing options...
Big Electric Cat Posted October 28, 2011 Report Share Posted October 28, 2011 There's a thread about this , which includes Glumpler's recipe from glazesharing blog: http://ceramicartsdaily.org/community/topic/1423-making-kiln-furniture/ Link to comment Share on other sites More sharing options...
Kabe Posted October 30, 2011 Author Report Share Posted October 30, 2011 There's a thread about this , which includes Glumpler's recipe from glazesharing blog: http://ceramicartsda...kiln-furniture/ Thanks Herb, I will try the recipe and see how it goes. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.