My bisque ware which I subsequently smoke fire is naturally not fired higher than 950C. I have been trying to attain an ultramarine blue which would contrast nicely with the deep black of the smoke firing. But because of the low temperature, I find that using a cobalt slip does not fully develop the colour. Does anyone have any idea how I could achieve a deeper blue slip?

Share this post


Link to post
Share on other sites

You could try mason stains or underglazes.

 

 

Thanks Chris. I must admit that I have never tried mason stains, but that might well be the way to go. Presumably I could add them to a slip in the usual way?

 

 

 

Share this post


Link to post
Share on other sites

Visit the mason website, look at the color charts and select stain that is recommended for use in a clay body.

The blues I have used get darker the higher they are fired. Your base clay color for the slip should be very white.

I just mix clay, water and stain in my studio blender ... but I am sure others have actual recipes.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×