Bob Coyle Posted June 1, 2015 Report Share Posted June 1, 2015 Here is a recipe for a tenmoku glaze for cone 5-6 oxidation. The glaze is very forgiving and gives good coverage when brushed at about 60% solids. It is hard to see in the pictures but there are iron red spots in the glaze. I can't remember where I got this glaze... probably Roy or Cushing. I decided to try it as a single fire glaze to see how it compared with bisque fired. I brushed it on the leather hard clay and let it dry, then fired it with the ordinary cone 5 cycle I use. I really couldn't see any difference between the two types of glaze applications. I use MR-5 and Speckled Buff from Laguna. I thought the Speckled buff might give me a different surface, but it didn't I don't make table ware so I don't know how this would hold up. There is nothing much in it that should cause toxicity problems. I really like the appearance of this glaze, but my customers don't. Pots with this glaze seem to sell last, so I backed off of using it mostly. I made some up for a class and ran these test tiles to see how a single fire would work. Component % Flint 25 Neph Sy 17 EPK 17 RIO 10 Gerstly Borate 08 Talc 08 Dolomite 08 Bone Ash 07 Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.