  1. Thank you! Its quite a learning experience but i really like it.
  2. Hi, I am using store bought liquid slip and plaster molds. Un-molding after leather hard and just letting air dry, usually 24 hours. This is an example and they all have multiple cracks like this. The more I do the more I research and the last slip i bought was super thick so i thinned it with just water and just discovered that was not good. Do you think this is why it is cracking?
  3. Hi, I am new to making ceramics and I need some help. After taking my clay out of the molds they look good but when they are dry and ready to kiln I notice that they are cracked. I cannot figure out why. Please help.
×
×