  1. I found it on the control box lid. As I have gone about the repair myself... I adjusted it and the wheel works great. I chosen this Creative Industry wheel over a newer Pacafica wheel just because the size of the motor. JohnnyK my email is demargoix@hotmail.com... Thank you all
  2. I am the proud new owner to a Creative Industries HP wheel. I understand it is not supported by the factory people any more. Is there a PFD of a service manual that someone has. The wheel works well except the pedal does not always stop the wheel. It has to be in the control but I need to how to open it for service... Thanks if you can help me out....
×
×