  1. Thanks for the info, much appreciated
  2. I recently learned about kiln maintenance and found that I need a sitter gauge to make sure I'm firing to the right temp. I bought my kiln second hand so I had no idea I was supposed to have one. My question is, are all gauges the same? Or should I buy one from my kiln & sitter manufacturer?
  3. I fire to 05-04 regularly and never see slumping. However I've heard that ur firing schedule can make a difference with slumping. I had problems at 6 and got the advice later to do a longer firing schedule. Haven't tried it out yet. At the low temp ur going for I wouldn't be very worried about slumping, but I agree with the other suggestions here, horizontal with supports is probably the way to go just to b safe.
×
×